1.
Artigo em Inglês | MEDLINE | ID: mdl-38300439

RESUMO

In orthopedic and dental surgery, the implantation of biomaterials within the bone to restore the integrity of the treated organ has become a standard procedure. Their long-term stability relies on the osseointegration phenomena, where bone grows onto and around metallic implants, creating a bone-implant interface. Bone is a highly hierarchical material that evolves spatially and temporally during this healing phase. A deeper understanding of its biomechanical characteristics is needed, as they are determinants for surgical success. In this context, we propose a multiscale homogenization model to evaluate the effective elastic properties of bone as a function of the distance from the implant, based on the tissue's structure and composition at lower scales. The model considers three scales: hydroxyapatite foam (nanoscale), ultrastructure (microscale), and tissue (mesoscale). The elastic properties and the volume fraction of the elementary constituents of bone matrix (mineral, collagen, and water), the orientation of the collagen fibril relative to the implant surface, and the mesoscale porosity constitute the input data of the model. The effect of a spatiotemporal variation in the collagen fibrils' orientation on the bone anisotropic properties in the proximity of the implant was investigated. The findings revealed a strong variation of the components of the effective elasticity tensor of the bone as a function of the distance from the implant. The effective elasticity appears to be primarily sensitive to the porosity (mesoscale) rather than to the collagen fibrils' orientation (sub-micro scale). However, the orientation of the fibrils has a significant influence on the isotropy of the bone. When analyzing the symmetry properties of the effective elasticity tensor, the ratio between the isotropic and hexagonal components is determined by a combination of the porosity and the fibrils' orientation. A decrease in porosity leads to a decrease in bone isotropy and, in turn, an increase in the impact of the fibrils' orientation. These results demonstrate that the collagen fibril orientation should be taken into account to properly describe the effective elastic anisotropy of bone at the organ scale.

2.
J Mech Behav Biomed Mater ; 141: 105787, 2023 05.
Artigo em Inglês | MEDLINE | ID: mdl-36989873

RESUMO

While cementless implants are now widely used clinically, implant debonding still occur and is difficult to anticipate. Assessing the biomechanical strength of the bone-implant interface can help improving the understanding of osseointegration phenomena and thus preventing surgical failures. A dedicated and standardized implant model was considered. The samples were tested using a mode III cleavage device to assess the mechanical strength of the bone-implant interface by combining experimental and numerical approaches. Four rough (Sa = 24.5 µm) osseointegrated coin-shaped implants were left in sheep cortical bone during 15 weeks of healing time. Each sample was experimentally rotated at 0.03°/sec until complete rupture of the interface. The maximum values of the torque were comprised between 0.48 and 0.72 N m, while a significant increase of the normal force from 7-12 N to 31-43 N was observed during the bone-implant interface debonding, suggesting the generation of bone debris at the bone-implant interface. The experimental results were compared to an isogeometric finite element model describing the adhesion and debonding phenomena through a modified Coulomb's law, based on a varying friction coefficient to represent the transition from an unbroken to a broken bone-implant interface. A good agreement was found between numerical and experimental torques, with numerical friction coefficients decreasing from 8.93 to 1.23 during the bone-implant interface rupture, which constitutes a validation of this model to simulate the debonding of an osseointegrated bone-implant interface subjected to torsion.


Assuntos
Prótese Ancorada no Osso , Implantes Dentários , Animais , Ovinos , Osseointegração , Fenômenos Mecânicos , Interface Osso-Implante , Próteses e Implantes , Análise de Elementos Finitos , Fenômenos Biomecânicos
3.
Matrix Biol ; 115: 32-47, 2023 01.
Artigo em Inglês | MEDLINE | ID: mdl-36435426

RESUMO

The specific viscoelastic mechanical properties of Achilles tendons are highly dependent on the structural characteristics of collagen at and between all hierarchical levels. Research has been conducted on the deformation mechanisms of positional tendons and single fibrils, but knowledge about the coupling between the whole tendon and nanoscale deformation mechanisms of more commonly injured energy-storing tendons, such as Achilles tendons, remains sparse. By exploiting the highly periodic arrangement of tendons at the nanoscale, in situ loading of rat Achilles tendons during small-angle X-ray scattering acquisition was used to investigate the collagen structural response during load to rupture, cyclic loading and stress relaxation. The fibril strain was substantially lower than the applied tissue strain. The fibrils strained linearly in the elastic region of the tissue, but also exhibited viscoelastic properties, such as an increased stretchability and recovery during cyclic loading and fibril strain relaxation during tissue stress relaxation. We demonstrate that the changes in the width of the collagen reflections could be attributed to strain heterogeneity and not changes in size of the coherently diffracting domains. Fibril strain heterogeneity increased with applied loads and after the toe region, fibrils also became increasingly disordered. Additionally, a thorough evaluation of radiation damage was performed. In conclusion, this study clearly displays the simultaneous structural response and adaption of the collagen fibrils to the applied tissue loads and provide novel information about the transition of loads between length scales in the Achilles tendon.


Assuntos
Tendão do Calcâneo , Ratos , Animais , Tendão do Calcâneo/fisiologia , Fenômenos Biomecânicos , Colágeno/química , Matriz Extracelular
4.
Med Biol Eng Comput ; 60(11): 3281-3293, 2022 Nov.
Artigo em Inglês | MEDLINE | ID: mdl-36169903

RESUMO

Inserting a titanium implant in the bone tissue may modify its physiological loading and therefore cause bone resorption, via a phenomenon called stress-shielding. The local stress field around the bone-implant interphase (BII) created under shear loading may be influenced by different parameters such as the bone-implant contact (BIC) ratio, the bone Young's modulus, the implant roughness and the implant material. A 2-D finite element model was developed to model the BII and evaluate the impact of the aforementioned parameters. The implant roughness was described by a sinusoidal function (height 2Δ, wavelength λ), and different values of the BIC ratio were simulated. A heterogeneous distribution of the maximum shear stress was evidenced in the periprosthetic bone tissue, with high interfacial stress for low BIC ratios and low implant roughness and underloaded regions near the roughness valleys. Both phenomena may lead to stress-shielding-related effects, which were concentrated within a distance lower than 0.8λ from the implant surface. Choosing an implant material with mechanical properties matching those of bone tissue leads to a homogenized shear stress field and could help to prevent stress-shielding effects. Finally, the equivalent shear modulus of the BII was derived to replace its complex behavior with a simpler analytical model in future studies. Schematic illustrations of the 2-D finite element model used in the present study and spatial variation of the maximal shear stress in the periprosthetic bone tissue for different implant roughness and bone-implant contact ratios.


Assuntos
Implantes Dentários , Titânio , Fenômenos Biomecânicos , Osso e Ossos , Análise de Elementos Finitos , Interfase , Osseointegração/fisiologia , Estresse Mecânico
5.
Front Bioeng Biotechnol ; 10: 911866, 2022.
Artigo em Inglês | MEDLINE | ID: mdl-35782510

RESUMO

Neutron tomography has emerged as a promising imaging technique for specific applications in bone research. Neutrons have a strong interaction with hydrogen, which is abundant in biological tissues, and they can penetrate through dense materials such as metallic implants. However, in addition to long imaging times, two factors have led to challenges in running in situ mechanical characterization experiments on bone tissue using neutron tomography: 1) the high water content in specimens reduces the visibility of internal trabecular structures; 2) the mechanical properties of bone are dependent on the hydration state of the tissue, with drying being reported to cause increased stiffness and brittleness. This study investigates the possibility of improving image quality in terms of neutron transmission and contrast between material phases by drying and rehydrating in heavy water. Rat tibiae and trabecular bovine bone plugs were imaged with neutron tomography at different hydration states and mechanical testing of the bone plugs was carried out to assess effects of drying and rehydration on the mechanical properties of bone. From analysis of image histograms, it was found that drying reduced the contrast between bone and soft tissue, but the contrast was restored with rehydration. Contrast-to-noise ratios and line profiles revealed that the contrast between bone tissue and background was reduced with increasing rehydration duration but remained sufficient for identifying internal structures as long as no free liquid was present inside the specimen. The mechanical analysis indicated that the proposed fluid exchange protocol had no adverse effects on the mechanical properties.

6.
J Mech Behav Biomed Mater ; 130: 105201, 2022 06.
Artigo em Inglês | MEDLINE | ID: mdl-35385809

RESUMO

Calcium sulfate/hydroxyapatite (CaS/HA) biomaterials have been investigated for use in several orthopedic applications. However, the mechanical interactions between the composite of CaS/HA and bone at the microscale are still unknown. The aim of this study was to determine if and how augmentation with CaS/HA alters the fracture behavior of bone. Eleven cylinders of trabecular bone were drilled from human femoral heads and cleaned from bone marrow. Among them, five cylinders were injected with CaS/HA to generate composite specimens, while the others were kept intact. One extra specimen of pure CaS/HA was prepared. All specimens were compressed in situ using synchrotron X-ray tomography and imaged at ∼2% strain intervals. Structural properties were calculated from the images in unloaded state and mechanical properties were determined from the load-curves. CaS/HA alone displayed the highest peak force and stiffness and the lowest strain at fracture. All composite specimens had a higher peak force than the pure bone specimens and the composite specimens had higher toughness than the pure CaS/HA specimen. Furthermore, the fracture behavior was analyzed further to characterize the local deformations. The pure bone specimens presented damage in multiple trabeculae and the CaS/HA specimen displayed sharp transition in strains, with low strain in one load step and large cracks in the next. The composite specimens deformed uniformly, with the CaS/HA preventing tissue damage and the bone preventing cracks in the CaS/HA from propagating through the specimen. In conclusion, using tomography with in situ loading, it was possible to show how CaS/HA can help prevent bone tissue damage before global failure.


Assuntos
Durapatita , Fraturas Ósseas , Materiais Biocompatíveis , Osso e Ossos , Sulfato de Cálcio , Durapatita/química , Fraturas Ósseas/diagnóstico por imagem , Humanos , Sulfatos
7.
Phys Med Biol ; 66(13)2021 07 07.
Artigo em Inglês | MEDLINE | ID: mdl-34010812

RESUMO

The bone tissue formed at the contact interface with metallic implants, particularly its 3D microstructure, plays a pivotal role for the structural integrity of implant fixation. X-ray tomography is the classical imaging technique used for accessing microstructural information from bone tissue. However, neutron tomography has shown promise for visualising the immediate bone-metal implant interface, something which is highly challenging with x-rays due to large differences in attenuation between metal and biological tissue causing image artefacts. To highlight and explore the complementary nature of neutron and x-ray tomography, proximal rat tibiae with titanium-based implants were imaged with both modalities. The two techniques were compared in terms of visualisation of different material phases and by comparing the properties of the individual images, such as the contrast-to-noise ratio. After superimposing the images using a dedicated image registration algorithm, the complementarity was further investigated via analysis of the dual modality histogram, joining the neutron and x-ray data. From these joint histograms, peaks with well-defined grey value intervals corresponding to the different material phases observed in the specimens were identified and compared. The results highlight differences in how neutrons and x-rays interact with biological tissues and metallic implants, as well as the benefits of combining both modalities. Future refinement of the joint histogram analysis could improve the segmentation of structures and tissues, and yield novel information about specimen-specific properties such as moisture content.


Assuntos
Processamento de Imagem Assistida por Computador , Tomografia Computadorizada por Raios X , Animais , Osso e Ossos/diagnóstico por imagem , Metais , Nêutrons , Ratos
8.
Phys Med Biol ; 66(10)2021 05 04.
Artigo em Inglês | MEDLINE | ID: mdl-33831846

RESUMO

Bone properties and especially its microstructure around implants are crucial to evaluate the osseointegration of prostheses in orthopaedic, maxillofacial and dental surgeries. Given the intrinsic heterogeneous nature of the bone microstructure, an ideal probing tool to understand and quantify bone formation must be spatially resolved. X-ray imaging has often been employed, but is limited in the presence of metallic implants, where severe artifacts generally arise from the high attenuation of metals to x-rays. Neutron tomography has recently been proposed as a promising technique to study bone-implant interfaces, thanks to its lower interaction with metals. The aim of this study is to assess the potential of neutron tomography for the characterisation of bone tissue in the vicinity of a metallic implant. A standardised implant with a bone chamber was implanted in rabbit bone. Four specimens were imaged with neutron tomography and subsequently compared to non-decalcified histology to stain soft and mineralised bone tissues, used here as a ground-truth reference. An intensity-based image registration procedure was performed to place the 12 histological slices within the corresponding 3D neutron volume. Significant correlations (p < 0.01) were obtained between the two modalities for the bone-implant contact (BIC) ratio (R = 0.77) and the bone content inside the chamber (R = 0.89). The results indicate that mineralised bone tissue can be reliably detected by neutron tomography. However, theBICratio and bone content were found to be overestimated with neutron imaging, which may be explained by its sensitivity to non-mineralised soft tissues, as revealed by histological staining. This study highlights the suitability of neutron tomography for the analysis of the bone-implant interface. Future work will focus on further distinguishing soft tissues from bone tissue, which could be aided by the adoption of contrast agents.


Assuntos
Interface Osso-Implante , Implantes Dentários , Animais , Nêutrons , Osseointegração , Próteses e Implantes , Coelhos , Titânio , Tomografia Computadorizada por Raios X , Microtomografia por Raio-X
9.
Bone ; 145: 115849, 2021 04.
Artigo em Inglês | MEDLINE | ID: mdl-33454374

RESUMO

Fetal immobilization affects skeletal development and can lead to severe malformations. Still, how mechanical load affects embryonic bone formation is not fully elucidated. This study combines mechanobiology, image analysis and developmental biology, to investigate the structural effects of muscular loading on embryonic long bones. We present a novel approach involving a semi-automatic workflow, to study the spatial and temporal evolutions of both hard and soft tissues in 3D without any contrast agent at micrometrical resolution. Using high-resolution phase-contrast-enhanced X-ray synchrotron microtomography, we compare the humeri of Splotch-delayed embryonic mice lacking skeletal muscles with healthy littermates. The effects of skeletal muscles on bone formation was studied from the first stages of mineral deposition (Theiler Stages 23 and 24) to just before birth (Theiler Stage 27). The results show that muscle activity affects both growth plate and mineralized regions, especially during early embryonic development. When skeletal muscles were absent, there was reduced mineralization, altered tuberosity size and location, and, at early embryonic stages, decreased chondrocyte density, size and elongation compared to littermate controls. The proposed workflow enhances our understanding of mechanobiology of early bone formation and could be implemented for the study of other complex biological tissues.


Assuntos
Lâmina de Crescimento , Osteogênese , Animais , Osso e Ossos , Condrócitos , Feminino , Camundongos , Gravidez , Microtomografia por Raio-X
10.
Adv Sci (Weinh) ; 7(21): 2002524, 2020 Nov.
Artigo em Inglês | MEDLINE | ID: mdl-33173750

RESUMO

Long bone mineralization occurs through endochondral ossification, where a cartilage template mineralizes into bone-like tissue with a hierarchical organization from the whole bone-scale down to sub-nano scale. Whereas this process has been extensively studied at the larger length scales, it remains unexplored at some of the smaller length scales. In this study, the changes in morphology, composition, and structure during embryonic mineralization of murine humeri are investigated using a range of high-resolution synchrotron-based imaging techniques at several length scales. With micro- and nanometer spatial resolution, the deposition of elements and the shaping of mineral platelets are followed. Rapid mineralization of the humeri occurs over approximately four days, where mineral to matrix ratio and calcium content in the most mineralized zone reach adult values shortly before birth. Interestingly, zinc is consistently found to be localized at the sites of ongoing new mineralization. The mineral platelets in the most recently mineralized regions are thicker, longer, narrower, and less aligned compared to those further into the mineralized region. In summary, this study demonstrates a specific spatial distribution of zinc, with highest concentration where new mineral is being deposited and that the newly formed mineral platelets undergo slight reshaping and reorganization during embryonic development.

11.
Med Eng Phys ; 84: 60-67, 2020 10.
Artigo em Inglês | MEDLINE | ID: mdl-32977923

RESUMO

Titanium implants are widely used in dental and orthopedic surgeries. Osseointegration phenomena lead to direct contact between bone tissue and the implant surface. The quality of the bone-implant interface (BII), resulting from the properties of newly formed bone, determines the implant stability. This study investigates the BII properties using a dedicated in vivo implant model consisting of a coin-shaped Ti-6Al-4V implant inserted in a rabbit femur for 10 weeks. A gap created below the implant was filled with newly formed bone tissue after healing. The properties of mature and newly formed bone tissues were compared using: i) Raman spectroscopy to assess the nanoscale compositional bone properties and ii) nanoindentation to quantify microscale elastic properties in site-matched regions. The mineral-to-matrix ratio, crystallinity (mineral size and lattice order), and the collagen cross-link ratio were significantly lower in newly formed bone tissue (e.g., a mineral-to-matrix ratio of 9.3 ± 0.5 for proline 853 cm-1) compared to mature bone (15.6 ± 1). Nanoindentation measurements gave Young's modulus of 12.8 ± 1.8 GPa for newly formed bone and 15.7 ± 2.3 GPa for mature bone. This multimodal and multiscale approach leads to a better understanding of osseointegration phenomena.


Assuntos
Interface Osso-Implante , Implantes Dentários , Animais , Osseointegração , Coelhos , Análise Espectral Raman , Propriedades de Superfície , Titânio
12.
Acta Biomater ; 116: 391-399, 2020 10 15.
Artigo em Inglês | MEDLINE | ID: mdl-32937205

RESUMO

A better understanding of bone nanostructure around the bone-implant interface is essential to improve longevity of clinical implants and decrease failure risks. This study investigates the spatio-temporal evolution of mineral crystal thickness and plate orientation in newly formed bone around the surface of a metallic implant. Standardized coin-shaped titanium implants designed with a bone chamber were inserted into rabbit tibiae for 7 and 13 weeks. Scanning measurements with micro-focused small-angle X-ray scattering (SAXS) were carried out on newly formed bone close to the implant and in control mature cortical bone. Mineral crystals were thinner close to the implant (1.8 ± 0.45 nm at 7 weeks and 2.4 ± 0.57 nm at 13 weeks) than in the control mature bone tissue (2.5 ± 0.21 nm at 7 weeks and 2.8 ± 0.35 nm at 13 weeks), with increasing thickness over healing time (+30 % in 6 weeks). These results are explained by younger bone close to the implant, which matures during osseointegration. Thinner mineral crystals parallel to the implant surface within the first 100 µm indicate that the implant affects the ultrastructure of neighbouring bone , potentially due to heterogeneous interfacial stresses, and suggest a longer maturation process of bone tissue and difficulty in binding to the metal. The bone growth kinetics within the bone chamber was derived from the spatio-temporal evolution of bone tissue's nanostructure, coupled with microtomographic imaging. The findings indicate that understanding mineral crystal thickness or plate orientation can improve our knowledge of osseointegration.


Assuntos
Interface Osso-Implante , Implantes Dentários , Animais , Durapatita , Osseointegração , Coelhos , Espalhamento a Baixo Ângulo , Propriedades de Superfície , Titânio , Difração de Raios X
13.
J Biomech Eng ; 142(12)2020 12 01.
Artigo em Inglês | MEDLINE | ID: mdl-32909597

RESUMO

Titanium implants are widely used in dental and orthopedic surgeries. However, implant failures still occur because of a lack of implant stability. The biomechanical properties of bone tissue located around the implant need to be assessed to better understand the osseointegration phenomena and anticipate implant failure. The aim of this study was to explore the spatiotemporal variation of the microscopic elastic properties of newly formed bone tissue close to an implant. Eight coin-shaped Ti6Al4V implants were inserted into rabbit tibiae for 7 and 13 weeks using an in vivo model allowing the distinction between mature and newly formed bone in a standardized configuration. Nanoindentation and micro-Brillouin scattering measurements were carried out in similar locations to measure the indentation modulus and the wave velocity, from which relative variations of bone mass density were extracted. The indentation modulus, the wave velocity and mass density were found to be higher (1) in newly formed bone tissue located close to the implant surface, compared to mature cortical bone tissue, and (2) after longer healing time, consistently with an increased mineralization. Within the bone chamber, the spatial distribution of elastic properties was more heterogeneous for shorter healing durations. After 7 weeks of healing, bone tissue in the bone chamber close to the implant surface was 12.3% denser than bone tissue further away. Bone tissue close to the chamber edge was 16.8% denser than in its center. These results suggest a bone spreading pathway along tissue maturation, which is confirmed by histology and consistent with contact osteogenesis phenomena.


Assuntos
Ligas , Osseointegração , Titânio , Animais , Interface Osso-Implante , Próteses e Implantes , Coelhos
14.
Sci Rep ; 10(1): 13788, 2020 08 14.
Artigo em Inglês | MEDLINE | ID: mdl-32796859

RESUMO

To comprehend the most detrimental characteristics behind bone fractures, it is key to understand the material and tissue level strain limits and their relation to failure sites. The aim of this study was to investigate the three-dimensional strain distribution and its evolution during loading at the sub-trabecular level in trabecular bone tissue. Human cadaver trabecular bone samples were compressed in situ until failure, while imaging with high-resolution synchrotron radiation X-ray tomography. Digital volume correlation was used to determine the strains inside the trabeculae. Regions without emerging damage were compared to those about to crack. Local strains in close vicinity of developing cracks were higher than previously reported for a whole trabecular structure and similar to those reported for single isolated trabeculae. Early literature on bone fracture strain thresholds at the tissue level seem to underestimate the maximum strain magnitudes in trabecular bone. Furthermore, we found lower strain levels and a reduced ability to capture detailed crack-paths with increased image voxel size. This highlights the dependence between the observed strain levels and the voxel size and that high-resolution is needed to investigate behavior of individual trabeculae. Furthermore, low trabecular thickness appears to be one predictor of developing cracks. In summary, this study investigated the local strains in whole trabecular structure at sub-trabecular resolution in human bone and confirmed the high strain magnitudes reported for single trabeculae under loading and, importantly extends its translation to the whole trabecular structure.


Assuntos
Osso Esponjoso/fisiopatologia , Fraturas de Estresse/fisiopatologia , Estresse Mecânico , Síncrotrons , Tomografia Computadorizada por Raios X/métodos , Osso e Ossos/fisiopatologia , Elasticidade/fisiologia , Fraturas de Estresse/diagnóstico , Humanos , Coluna Vertebral/fisiopatologia , Suporte de Carga/fisiologia
15.
Artigo em Inglês | MEDLINE | ID: mdl-32850760

RESUMO

Better understanding of the local deformation of the bone network around metallic implants subjected to loading is of importance to assess the mechanical resistance of the bone-implant interface and limit implant failure. In this study, four titanium screws were osseointegrated into rat tibiae for 4 weeks and screw pullout was conducted in situ under x-ray microtomography, recording macroscopic mechanical behavior and full tomographies at multiple load steps before failure. Images were analyzed using Digital Volume Correlation (DVC) to access internal displacement and deformation fields during loading. A repeatable failure pattern was observed, where a ∼300-500 µm-thick envelope of bone detached from the trabecular structure. Fracture initiated close to the screw tip and propagated along the implant surface, at a distance of around 500 µm. Thus, the fracture pattern appeared to be influenced by the microstructure of the bone formed closely around the threads, which confirmed that the model is relevant for evaluating the effect of pharmacological treatments affecting local bone formation. Moreover, cracks at the tibial plateau were identified by DVC analysis of the tomographic images acquired during loading. Moderate strains were first distributed in the trabecular bone, which localized into higher strains regions with subsequent loading, revealing crack-formation not evident in the tomographic images. The in situ loading methodology followed by DVC is shown to be a powerful tool to study internal deformation and fracture behavior of the newly formed bone close to an implant when subjected to loading. A better understanding of the interface failure may help improve the outcome of surgical implants.

16.
J Biomed Mater Res B Appl Biomater ; 106(1): 104-111, 2018 Jan.
Artigo em Inglês | MEDLINE | ID: mdl-27875027

RESUMO

New fusionless devices are being developed to get over the limits of actual spinal surgical treatment, based on arthrodesis. However, due to their recentness, no standards exist to test and validate those devices, especially concerning the wear. A new tribological first approach to the definition of an in vitro wear protocol to study wear of flexible and sliding spinal devices is presented in this article, and was applied to a new concept. A simplified synthetic spine portion (polyethylene) was developed to reproduce a simple supra-physiological spinal flexion (10° between two vertebrae). The device studied with this protocol was tested in wet environment until 1 million cycles (Mc). We obtained an encouraging estimated wear volume of same order of magnitude compared to similar devices. An associated finite element (FE) numerical model has permitted to access contact information and study the effect of misalignment of one screw. First results could point out how to improve the design and suggest that a vertical misalignment of a screw (under or over-screwing) has more impact than a horizontal one. © 2016 Wiley Periodicals, Inc. J Biomed Mater Res Part B: Appl Biomater, 106B: 104-111, 2018.


Assuntos
Implantes Experimentais , Modelos Biológicos , Coluna Vertebral , Análise de Elementos Finitos , Humanos
17.
Artigo em Inglês | MEDLINE | ID: mdl-30719433

RESUMO

Long-term stability of endosseous implants depends on successful bone formation, ingrowth and adaptation to the implant. Specifically, it will define the mechanical properties of the newly formed bone-implant interface. 3D imaging during mechanical loading tests (in situ loading) can improve the understanding of the local processes leading to bone damage and failure. In this study, titanium screws were implanted into rat tibiae and were allowed to integrate for 4 weeks with or without the addition of the growth factor Bone Morphogenetic Protein and the bisphosphonate Zoledronic Acid. Samples were subjected to in situ pullout using high-resolution synchrotron x-ray tomography at the Tomcat beamline (SLS, PSI, Switzerland) at 30 keV with 25 ms exposure time, resulting in a total acquisition time of 45 s per scan, with a 3.6 µm isotropic voxel size. Using a custom-made loading device positioned inside the beamline, screws were pulled out with 0.05 mm increment, acquiring multiple scans until rupture of the sample. The in situ loading protocol was adapted to ensure short imaging time, which enabled multiple samples to be tested with short loading steps, while keeping the total testing time low and reducing dose deposition. Higher trabecular bone content was quantified in the surrounding of the screw in the treated groups, which correlated with increased mechanical strength and stiffness. Differences in screw implantation, such as contact between threads and cortex as well as minor tilt of the screw were also correlated to the mechanical parameters. In situ loading enabled the investigation of crack propagation during the pullout, highlighting the mechanical behavior of the interface. Three typical crack types were observed: (1) rupture at the interface of trabecular and cortical bone tissues, close to the screw, (2) large crack inside the cortex connected to the implant, and (3) first failure away from the screw with cracks propagating toward the screw-bone interface. Mechanical properties of in vivo integrated bone-metal screws rely on a combination of multiple parameters that are difficult to identify and separate one from the other.

18.
J Mech Behav Biomed Mater ; 75: 271-278, 2017 11.
Artigo em Inglês | MEDLINE | ID: mdl-28759839

RESUMO

Metallic implants are commonly used as surgical treatments for many orthopedic conditions. The long-term stability of implants relies on an adequate integration with the surrounding bone. Unsuccessful integration could lead to implant loosening. By combining mechanical loading with high-resolution 3D imaging methods, followed by image analysis such as Digital Volume Correlation (DVC), we aim at evaluating ex vivo the mechanical resistance of newly formed bone at the interface. X-rays tomography is commonly used to image bone but induces artefacts close to metallic components. Utilizing a different interaction with matter, neutron tomography is a promising alternative but has not yet been used in studies of bone mechanics. This work demonstrates that neutron tomography during in situ loading is a feasible tool to characterize the mechanical response of bone-implant interfaces, especially when combined with DVC. Experiments were performed where metal screws were implanted in rat tibiae during 4 weeks. The screws were pulled-out while the samples were sequentially imaged in situ with neutron tomography. The images were analyzed to quantify bone ingrowth around the implants. DVC was used to track the internal displacements and calculate the strain fields in the bone during loading. The neutron images were free of metal-related artefacts, which enabled accurate quantification of bone ingrowth on the screw (ranging from 60% to 71%). DVC allowed successful identification of the deformation and cracks that occurred during mechanical loading and led to final failure of the bone-implant interface.


Assuntos
Osso e Ossos/fisiologia , Interface Osso-Implante/diagnóstico por imagem , Metais , Animais , Parafusos Ósseos , Masculino , Nêutrons , Ratos , Ratos Sprague-Dawley , Tomografia Computadorizada por Raios X
19.
Bone ; 103: 295-301, 2017 Oct.
Artigo em Inglês | MEDLINE | ID: mdl-28739417

RESUMO

Metal implants, in e.g. joint replacements, are generally considered to be a success. As mechanical stability is important for the longevity of a prosthesis, the biological reaction of the bone to the mechanical loading conditions after implantation and during remodelling determines its fate. The bone reaction at the implant interface can be studied using high-resolution imaging. However, commonly used X-ray imaging suffers from image artefacts in the close proximity of metal implants, which limit the possibility to closely examine the bone at the bone-implant interface. An alternative ex vivo 3D imaging method is offered by neutron tomography. Neutrons interact with matter differently than X-rays; therefore, this study explores if neutron tomography may be used to enrich studies on bone-implant interfaces. A stainless steel screw was implanted in a rat tibia and left to integrate for 6weeks. After extracting the tibia, the bone-screw construct was imaged using X-ray and neutron tomography at different resolutions. Artefacts were visible in all X-ray images in the close proximity of the implant, which limited the ability to accurately quantify the bone around the implant. In contrast, neutron images were free of metal artefacts, enabling full analysis of the bone-implant interface. Trabecular structural bone parameters were quantified in the metaphyseal bone away from the implant using all imaging modalities. The structural bone parameters were similar for all images except for the lowest resolution neutron images. This study presents the first proof-of-concept that neutron tomographic imaging can be used for ex-vivo evaluation of bone microstructure and that it constitutes a viable, new tool to study the bone-implant interface tissue remodelling.


Assuntos
Parafusos Ósseos , Interface Osso-Implante/diagnóstico por imagem , Imageamento Tridimensional/métodos , Nêutrons , Tomografia/métodos , Animais , Masculino , Ratos , Ratos Sprague-Dawley , Tomografia Computadorizada por Raios X
20.
PLoS One ; 10(10): e0127463, 2015.
Artigo em Inglês | MEDLINE | ID: mdl-26451947

RESUMO

The porcine model is frequently used during development and validation of new spinal devices, because of its likeness to the human spine. These spinal devices are frequently composed of pedicle screws with a reputation for stable fixation but which can suffer pullouts during preclinical implantation on young animals, leading to high morbidity. With a view to identifying the best choices to optimize pedicle screw fixation in the porcine model, this study evaluates ex vivo the impact of weight (age) of the animal, the level of the vertebrae (lumbar or thoracic) and the type of screw anchorage (mono- or bi-cortical) on pedicle screw pullouts. Among the 80 pig vertebrae (90- and 140-day-old) tested in this study, the average screw pullout forces ranged between 419.9N and 1341.2N. In addition, statistical differences were found between test groups, pointing out the influence of the three parameters stated above. We found that the the more caudally the screws are positioned (lumbar level), the greater their pullout resistance is, moreover, screw stability increases with the age, and finally, the screws implanted with a mono-cortical anchorage sustained lower pullout forces than those implanted with a bi-cortical anchorage. We conclude that the best anchorage can be obtained with older animals, using a lumbar fixation and long screws traversing the vertebra and inducing bi-cortical anchorage. In very young animals, pedicle screw fixations need to be bi-cortical and more numerous to prevent pullout.


Assuntos
Parafusos Pediculares , Animais , Vértebras Lombares/cirurgia , Suínos